K-Plate
Tin plate with superior corrosion
resistance to mild acid food products; must meet four (4) special
property tests : 1. Pickle lags 10 or less. 2. Tin crystal size ASTM 9
or larger. 3. ISV (iron solution value) 20 micro grams Fe or less. 4.
ATC (Alloy tin couple - American Can test) or AMP (Aerated Media
Polarization test) Avg. 0.050 micro amps/sq. cm. Or less – 95% 0.085 or
less. No test over 0.120. |
|
 |
|

|
|